Polymer Property : Rear Barrel Temperature = 530 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 291 °C
530 - 555 °F
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman.
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6
Description: Abrasion Resistant Nylon 6Information provided by Wellman.
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66
Description: Medium Impact Nylon 66Information provided by Wellman.
Rear Barrel Temperature 277 - 293 °C
530 - 560 °F
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..