| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized
Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade
Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond..
|
|||
| Mold Temperature | 76.7 - 121 °C | 170 - 250 °F | |
|
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat
Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate
Information provided by Ravago.
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Mold Temperature | 76.7 - 100 °C | 170 - 212 °F | Average value: 95.9 °C Grade Count:6 |
|
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1212FR Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1212FRRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1212FRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1510R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1510UV Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 110 °C | 170 - 230 °F | |
|
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
|
|||
| Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
|
Star Plastics PC1212R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
|
|||
| Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
|
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 76.7 - 121 °C | 170 - 250 °F | |
|
Polymer Resources PPX/NY GP2 Modified PPO, Medium Heat PPX/Nylon 6,6 Alloy
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
|
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||