Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Cycolac® MG47 ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Cycolac® MG47N ABS
Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific)
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific)
High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific)
Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC 3
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
PLC code 3; UL 746A
SABIC Innovative Plastics Lexan® PPC4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 925AU PC
Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific)
Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 945U PC (Asia Pacific)
Lexan* 945U Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing additio..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific)
Transparent, clear and colors, high viscosity, flame retardant with exceptional surface.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 38.6 mm/min Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 67.6 mm/min Grade Count:6
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL746A
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin
Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
LG Chemical AF308 ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific)
PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics Valox® 745 PBT
30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks.
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min
3.15 - 5.91 in/min
UL 746A
SABIC Innovative Plastics NORYL PX1543 PPE+PS (Asia Pacific)
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min

@Thickness 3.00 mm
3.15 - 5.91 in/min

@Thickness 0.118 in
UL Rating PLC 3 (80-150 mm/min.)
Covestro Makrolon® 6485 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was ..
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min

@Thickness 1.50 mm
3.15 - 5.91 in/min

@Thickness 0.0591 in
UL Rating PLC 3 (80-150 mm/min.)
Covestro Makrolon® 6555 Polycarbonate, Injection Grade
Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a..