Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PCSF-FR Polycarbonate, 5% Glass Reinforced Structural Foam Grade Polycarbonate, 5% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing cond.. |
|||
Mold Temperature | 76.7 - 121 °C | 170 - 250 °F | |
Polymer Resources PPX/NY GP2 PPO/Nylon 66 Alloy, Medium Heat Polyphenylene Oxide/Nylon 66 Alloy , General Purpose, Medium HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive.. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 76.7 - 100 °C | 170 - 212 °F | Average value: 95.9 °C Grade Count:6 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1212FRRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC701 Molding Grade PC with release Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 104 °C | 170 - 220 °F | |
Star Plastics PC743 Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Mold Temperature | 76.7 - 110 °C | 170 - 230 °F | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Entec Hylex® P1310FR Polycarbonate Information provided by Ravago |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Entec Hylex® P1010FR Polycarbonate Information provided by Ravago. |
|||
Mold Temperature | 76.7 - 82.2 °C | 170 - 180 °F | Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products. |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Mold Temperature | 76.7 - 93.3 °C | 170 - 200 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 76.7 - 98.9 °C | 170 - 210 °F | |
Polymer Resources PPX-FRG10 Modified PPO, UL 94 V-1, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |