Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.57 g/cc | 1.57 g/cc | ASTM D792 |
Water Absorption | 0.50 % | 0.50 % | ASTM D570 |
Maximum Moisture Content | 0.090 | 0.090 | Injection Molding |
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0050 in/in @Thickness 0.126 in |
ASTM D955 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 122 | 122 | ASTM D785 |
Tensile Strength, Yield | 230 MPa @Thickness 3.20 mm |
33400 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
Elongation at Break | 2.0 % @Thickness 3.20 mm |
2.0 % @Thickness 0.126 in |
5mm/min; ASTM D638 |
Flexural Yield Strength | 329 MPa @Thickness 3.20 mm |
47600 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
Flexural Modulus | 14.27 GPa @Thickness 3.20 mm |
2069 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ASTM D696 |
Melting Point | 260 °C | 500 °F | ASTM D3418 |
Deflection Temperature at 0.46 MPa (66 psi) | 260 °C @Thickness 6.40 mm |
500 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C @Thickness 6.40 mm |
491 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
UL RTI, Electrical | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
UL RTI, Mechanical with Impact | 110 °C @Thickness >=0.750 mm |
230 °F @Thickness >=0.0295 in |
|
110 °C @Thickness >=1.50 mm |
230 °F @Thickness >=0.0591 in |
||
110 °C @Thickness >=3.00 mm |
230 °F @Thickness >=0.118 in |
||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
||
120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
||
Flammability, UL94 | HB @Thickness >=0.750 mm |
HB @Thickness >=0.0295 in |
|
HB @Thickness >=1.50 mm |
HB @Thickness >=0.0591 in |
||
HB @Thickness >=3.00 mm |
HB @Thickness >=0.118 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Dielectric Constant | 4.0 @Frequency 1.00e+6 Hz |
4.0 @Frequency 1.00e+6 Hz |
ASTM D150 |
Dielectric Strength | 25.0 kV/mm @Thickness 1.00 mm |
635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
15 - 30 sec @Thickness >=1.50 mm |
15 - 30 sec @Thickness >=0.0591 in |
||
15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
||
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
>= 120 arcs @Thickness 1.50 mm |
>= 120 arcs @Thickness 0.0591 in |
||
>= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
Front Barrel Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
Nozzle Temperature | 270 - 290 °C | 518 - 554 °F | Injection Molding |
Melt Temperature | 270 - 295 °C | 518 - 563 °F | Injection Molding |
Mold Temperature | 80.0 - 110 °C | 176 - 230 °F | Injection Molding |
Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |