Polymer Property : Rear Barrel Temperature = 260 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 270 °C
500 - 518 °F
NHEP Spectron™ E6666 Nylon 66, 30% Glass Fiber
Natural color. E6666 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati..
Rear Barrel Temperature 260 - 275 °C
500 - 527 °F
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Rear Barrel Temperature 260 - 275 °C
500 - 527 °F
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Rear Barrel Temperature 260 - 270 °C
500 - 518 °F
Injection Molding
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Rear Barrel Temperature 260 - 300 °C
500 - 572 °F
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE
NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi..
Rear Barrel Temperature 260 - 293 °C
500 - 560 °F
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled
33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc.
Rear Barrel Temperature 260 - 271 °C
500 - 520 °F
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
Rear Barrel Temperature 260 - 271 °C
500 - 520 °F
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
Rear Barrel Temperature 260 - 300 °C
500 - 572 °F
Injection Molding
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Injection Molding
LG Chemical LUPOY GP1006FM PC, Flame Retardant
Description: Injection Molding, PC, Flame RetardantApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Rear Barrel Temperature 260 - 282 °C
500 - 540 °F
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow
Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern..
Rear Barrel Temperature 260 - 270 °C
500 - 518 °F
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
Rear Barrel Temperature 260 - 270 °C
500 - 518 °F
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50
Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Aft-1. Region Temperature
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Aft-1. Region Temperature
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Aft-1. Region Temperature
Tisan TISLAMID® 66 Impact Modified Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Rear Barrel Temperature 260 - 282 °C
500 - 540 °F
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Rear Barrel Temperature 260 - 282 °C
500 - 540 °F
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Zone 1
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Zone 1
Eurostar Staramide AG5 PA66, 25% Glass Filled, Injection Molded
AG5 is a 25% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Rear Barrel Temperature 260 °C
500 °F
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Flame retardant, Thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 260 °C
500 °F
Beijing Chemical Industry KAIFA® M106N MPPO Resin
High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
Rear Barrel Temperature 260 - 290 °C
500 - 554 °F
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Rear Barrel Temperature 260 - 280 °C
500 - 536 °F
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
Rear Barrel Temperature 260 - 300 °C
500 - 572 °F
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..