Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0050 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
PolyOne Novablend™ 6602 Polyvinyl Chloride, Rigid (PVC, Rigid)
Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: ..
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific)
Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance.
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0020 - 0.0050 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
PTS PPE-LXS 314-10 PPE-HIPS, 10% Glass Filled
Typical Applications: Water industrial partsInformation provided by PTS LLC.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955 and ISO 294-4
Ravago Manufacturing Americas Hylon® N1233HL BK Nylon 6/6
Available in North America Filler: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantAuto Specifications: ..
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0040 - 0.0050 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Asia Pacific)
5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 2.00 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® CE15315 NC010 PBT &nbsp;(Unverified Data**)
Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Ravago Manufacturing Americas Hylon® N1035HHR Nylon 66, 35% Glass Filled &nbsp;(discontinued **)
Heat Stabilized, Hydrolysis Resistant in Automotive CoolantInformation provided by Ravago.
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0020 - 0.0050 in/in
<br>@Thickness 0.126 in
ASTM D955
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics NORYL V01525 PPE+HIPS
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES
LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM 2210K PEI
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics ULTEM 2310EPR PEI
30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12
LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0020 - 0.0050 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66
LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Ultem ATX102R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
on Tensile Bar; E2P method
Eurostar Staramide PF006IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide PF006IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X R2005-30V)Information provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Time 86400 sec
0.0030 - 0.0050 in/in
<br>@Time 24.0 hour
E2P method
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified
Data provided by Clariant Masterbatches
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant
Data provided by Clariant Masterbatches
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm
<br>@Thickness 3.00 mm
0.0040 - 0.0050 in/in
<br>@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
<br>@Thickness 3.20 mm
0.0030 - 0.0050 in/in
<br>@Thickness 0.126 in
ASTM D955
LG Chemical LUPOL GP2300 PP+GF30%
Description: Injection Molding, PP+GF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Copyright © lookpolymers.com All Rights Reserved