Polymer Property : UL RTI, Mechanical with Impact = 230 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
PolyOne Maxxam™ FR PP FR 7B01 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
UL RTI, Mechanical with Impact 110 °C

@Thickness 0.710 mm
230 °F

@Thickness 0.0280 in
UL 746B
DuPont Performance Polymers Crastin® CE15315 BK010 PBT  (Unverified Data**)
Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® CE15315 NC010 PBT  (Unverified Data**)
Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical LUMID GP2151AF PA6+GF15%, Flame Retardant
Feature: Injection Molding, PA6+GF15%, Flame RetardantApplication: ConnectorsCAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
UL RTI, Mechanical with Impact 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant
Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant
Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin
Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical with Impact 110 °C

@Thickness >=2.00 mm
230 °F

@Thickness >=0.0787 in
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical LUPOY GN1006FMR PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, Transparency, Mold ReleaseApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin
Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=1.50 mm
230 °F

@Thickness >=0.0591 in
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin
Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=2.00 mm
230 °F

@Thickness >=0.0787 in
LG Chemical Lupoy NF1009F 08R Polycarbonate Resin
Description: LUPOY NF 1009F08R, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=2.00 mm
230 °F

@Thickness >=0.0787 in
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1302-10 Polycarbonate Resin
Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical with Impact 110 °C

@Thickness >=3.00 mm
230 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL746B
DSM Akulon® K223-KMV6 (GREY) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Mechanical with Impact 110 °C

@Thickness 0.750 mm
230 °F

@Thickness 0.0295 in
UL746B
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
ALL
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
UL RTI, Mechanical with Impact 110 °C

@Thickness 2.00 mm
230 °F

@Thickness 0.0787 in
ALL
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded
Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
UL RTI, Mechanical with Impact 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
ALL
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded
Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL746B
DSM Arnite® T06 200 (extrusion) PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
UL RTI, Mechanical with Impact 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
UL RTI, Mechanical with Impact 110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746B
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
UL RTI, Mechanical with Impact 110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL746B
DSM Arnite® T08 200 (extrusion) T08 200 PBT (European and Asian Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Mechanical with Impact 110 °C

@Thickness 0.750 mm
230 °F

@Thickness 0.0295 in
UL746B
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..