| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical ER451 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HI110 ABS, High Impact, Chemical Resistance
Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HI121U ABS
Feature: Injection Molding, Well Balanced Mechanical Properties, Good weatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemic..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS 403AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS 501S PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Food Holder, Food Container, Plastic Toy, Sheet or Film of Yot ReceptacleCAS: 9003-55-8Information provi..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI750L PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID SG2600B PA6+GF60%, General purpose, Good Surface
Feature: Injection Molding, PA6+GF60%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3200 PP+MF20%
Description: Injection Molding, PP+MF10%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3302 PP+MF30%
Description: Injection Molding, PP+MF30%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HF5254A PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HI5302R PP+MF30%, High Impact
Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Battery Case, Light CoverCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3156F Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided ..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3402 PP+MF40%
Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical SG175G ABS, Super Surface Gloss, High Flow
Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical XR401F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical KEYFLEX TO1075AR Olefin Type TPE
Description: Injection Molding, TPV, General Purpose, Soft TouchApplication: Automotive InteriorCAS: 9003-07-0, 9010-79-1, 64742-54-7 and 14807-96-6Information provided by LG Chemical
|
|||