| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability
Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI730 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI750L PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)
Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG ..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant
Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose
Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUMID HI1102B(W) PA66, High Impact
Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL EI5002L PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP1007F Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP2200 PP+GF20%
Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3202 PP+MF20%
Description: Injection Molding, PP+MF10%, General Purpose, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3300 PP+MF30%
Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HI5204H PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical ER461 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL GP3400S PP+MF40%
Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HF5157 PP+Rubber+MF, High Flow and Stiffness, High Impact
Description: Injection Molding, PP+Rubber+MF, High Flow and Stiffness, High Impact, Good Weatherability, Scratch ResistanceApplication: Automotive Exterior (Slim wall Bumper Fascia)Information provi..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL HM3102A PP+MF10%, High Impact
Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
|
LG Chemical MA201 ABS, Low Gloss
Feature: Injection Molding, Extrusion Molding, General Purpose, Low GlossApplication: Automotive Sheet, Semi-Conductor TrayCAS No. 9003-56-9Information provided by LG Chemical
|
|||