Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Mechanical without Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT  (Unverified Data**)
Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® S600F20 BK851 PBT  (Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical without Impact 120 °C

@Thickness >=0.750 mm
248 °F

@Thickness >=0.0295 in
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=3.00 mm
248 °F

@Thickness >=0.118 in
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=3.00 mm
248 °F

@Thickness >=0.118 in
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose
Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=0.750 mm
248 °F

@Thickness >=0.0295 in
LG Chemical LUPOL GP1000FC Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=1.60 mm
248 °F

@Thickness >=0.0630 in
LG Chemical Lupoy 1302-05 Polycarbonate Resin
Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main..
UL RTI, Mechanical without Impact 120 °C

@Thickness >=1.60 mm
248 °F

@Thickness >=0.0630 in
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical without Impact 120 °C

@Thickness >=2.50 mm
248 °F

@Thickness >=0.0984 in
LG Chemical Lupoy 1302-07 Polycarbonate Resin
Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical without Impact 120 °C

@Thickness >=2.00 mm
248 °F

@Thickness >=0.0787 in
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=2.00 mm
248 °F

@Thickness >=0.0787 in
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=3.00 mm
248 °F

@Thickness >=0.118 in
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness >=1.50 mm
248 °F

@Thickness >=0.0591 in
LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance
Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov..
UL RTI, Mechanical without Impact 120 °C

@Thickness >=3.00 mm
248 °F

@Thickness >=0.118 in
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin
Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
UL RTI, Mechanical without Impact 120 °C

@Thickness >=1.50 mm
248 °F

@Thickness >=0.0591 in
LG Chemical Lupoy 1303-07 Polycarbonate Resin
Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
UL RTI, Mechanical without Impact 120 °C

@Thickness >=2.50 mm
248 °F

@Thickness >=0.0984 in
LG Chemical LUPOY GP1006FL PC, Flame Retardant
Description: Injection Molding, PC, Flame Retardant, High FlowApplication: IT/OA, E&E Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.17 mm
248 °F

@Thickness 0.125 in
UL 746
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman.
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.17 mm
248 °F

@Thickness 0.125 in
UL 746
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman.
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL746B
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
UL RTI, Mechanical without Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL746B
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded
AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su..
UL RTI, Mechanical without Impact 120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL746B
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
UL RTI, Mechanical without Impact 120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
UL RTI, Mechanical without Impact 120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..