Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.57 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
PolyOne LubriOne™ NI-20GF/15T FR Polyamide 610 (Nylon 610)
Information provided by PolyOne
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Ovation Polymers Opnyl OP66GF50 Nylon 66
Nylon 66-Glass reinforced(50%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Ravago Manufacturing Americas Hylon® N1025HLFR Nylon 6/6, 25% Fiberglass, Heat Stabilized, Lubricated, Flame retardant (Cond)
Information provided by Ravago.
Specific Gravity 1.57 g/cc

@Temperature 23.0 °C
1.57 g/cc

@Temperature 73.4 °F
ASTM D792
Kingfa PBT-RG20 Flame Retardant, 20% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Kotec Carbotex KG-30F15 Polycarbonate, Wear Resistant, 30% Glass Fiber Reinforced
Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p..
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers
PA 66, 50% glass fibers, injection molding, heat-ageing stabilized
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Samsung Cheil Industries Infino® MKD-1015 PA, Glass Filled
Information provided by Samsung Cheil Industries.
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RX09411H PA 66
LNP* Thermocomp* RX09411H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare.
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D297, 15
Seals Eastern 7182B Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ Beige 1266E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 1266E is a beige color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH®..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. ..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. ..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. ..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good dist..
Specific Gravity 1.57 g/cc
1.57 g/cc
Trelleborg Commercial Neoprene® C722 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good dist..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8750 Concentrate Based In HDPE
DescriptionPOLYBATCH® B8750 is a specialty white masterbatch based in HDPE. This product has been designed to achieve optimum dispersion and excellent letdown mixing in blow molding applications. ..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
A. Schulman POLYBATCH™ White 8153/UV2 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 8153/UV2 is a white/UV masterbatch based in polyethylene. This product has been specifically engineered to provide dispersion and opacity at a competitive cost with good dist..
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D792
Asahi Kasei Thermylon® NSG-240A-C 50% Ceramic and Glass Fiber Reinforced
Information provided by Asahi Thermofil
Specific Gravity 1.57 g/cc
1.57 g/cc
ISO 1183/1
A. Schulman SCHULAMID® 66 GF50H 50% Glass Fiber Reinforced, Heat Stabilized 66
Information provided by A. Schulman.
Specific Gravity 1.57 g/cc
1.57 g/cc
Kuraray Genestar™ GR2300 Nylon, 30% Glass Filled
Standard V-0 Grade. Delivers increased fluidity and weld strength. Well suited for a wide range of electrical and electronic components.
Copyright © lookpolymers.com All Rights Reserved