Polymer Property : Front Barrel Temperature = 290 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Zone
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Front Barrel Temperature 240 - 290 °C
464 - 554 °F
Start Point: 270°C
Kingfa PC-S923 Modified PC
Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Injection Molding
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose
Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Injection Molding
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Injection Molding
LG Chemical LUMID SG4389B PA66+GF/MF38%
Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical
Front Barrel Temperature 275 - 290 °C
527 - 554 °F
Injection Molding
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and ..
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5000FQ General Purpose PC/ABS Alloy, Unreinforced, Excellent Flow
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
LG Chemical LUPOY HI-1002 High Impact Modified PC, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Start Point: 275°C
Kingfa JH710 G30 Flame Retardant & 30% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Start Point: 275°C
Kingfa PC-WT01 Weather Resistance PC
Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50
Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH50
Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Solvay TECHNYL® A 246M PA66, DRY
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay Technyl® A218GV33-BK 33% Glass Filled, Heat Stabilized, Hydrolysis Resistant, Black Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® SSD 330 KNF/E PA66, 15% glass filled, DRY
Description: Polyamide 66, reinforced with 33% of glass fiber, for injection molding specially stabilized to improves its resistance to automotive cooling liquids.Available in: Asia PacificProduct A..
Front Barrel Temperature 285 - 290 °C
545 - 554 °F
Solvay TECHNYL® A 216 PA66, DRY
Description: Unreinforced polyamide 66, medium viscosity, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: TECHNYL ® A 216 offers all of the primary propert..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Solvay TECHNYL® A 216T V33 Black 1 N PA66, 33% glass fiber, DRY
Description: Polyamide PA66 reinforced with 33% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, EuropeProduct Applications: TECHNYL® A 216T V33 BLACK 1N is used..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Zone 3
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Zone 3
Eurostar Staramide AG7K PA66, 35% Glass Filled, Injection Molded
AG7 is a Heat and Hydrolytically Stabilized, 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Zone
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Zone
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)  (discontinued **
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..