Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Voltage Arc-Tracking Rate, HVTR = 10.0 mm/min Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Cycolac® EX58F ABS
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 80.0 mm/min
0.394 - 3.15 in/min
Average value: 37.1 mm/min Grade Count:13
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS
High impact and ductility at 73F (23C) and -20F (-29C).
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific)
High impact and ductility at 73F (23C) and -20F (-29C).
High Voltage Arc-Tracking Rate, HVTR 10.0 - 50.0 mm/min
0.394 - 1.97 in/min
Average value: 32.7 mm/min Grade Count:4
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 38.6 mm/min Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min
<= 0.394 in/min
UL Rating PLC 0 (0-10 mm/min)
LG Chemical 65IH HIPS
High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical HIPS 403AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LI942 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUPOY GP1000HU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: Electric & Electronic (Housing, Components) For Suit caseCAS: 103598-77-2Information provided by LG Chemic..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical RS650 ABS
Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUPOY GP1000LG PC, Transparent
Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUPOY GP1000MD PC, Light Diffusion
Description: Injection Molding, PC, General Purpose, Light DiffusionApplication: IT/OA Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUPOY GP1000MR PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUPOY GP1000SW PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: Keypad for Mobile Phone, Automotive (Interior)CAS: 103598-77-2Information provided by LG Chemical
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min
<= 0.394 in/min
UL Rating PLC 0 (0-10 mm/min)
LG Chemical SG-950 Alphalac Polystyrene
High strength, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electr..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 310 PBT
Unreinforced, general purpose. Typical viscosity 5000-7000.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific)
Unreinforced, general purpose. Typical viscosity 5000-7000.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 325 PBT
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific)
General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific)
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 780 PBT
40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL 746A
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific)
15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min

@Thickness 3.00 mm
0.394 - 1.00 in/min

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL Rating PLC 1 (10-25.4 mm/min)
LG Chemical 402 AF Flame Retardant HIPS
NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t..
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved