Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : Lehmann & Voss & Co. > Category : Polyketone Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7197/BK PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7290 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7301 PEEK, unreinforced, laser markable Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7336/GY7016 PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7460/BL5019 PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7568/GY PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7719/BN PEEK, with glass fiber, easy flowing Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7751 PEEK, with carbon fiber, easy flowing Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7753/BL PEEK, unreinforced, easy flowing Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7777 PEEK, lubricant modified Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7786 PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7794/BL PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7852 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7907 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7938/GY PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7944 PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8053/EM/BL PEEK, with glass fiber, easy flowing Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8059 PEEK, lubricant modified, easy flowing Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8102 PEEK, with PTFE, lubricant modified, easy flowing Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8135/VI PEEK, unreinforced, easy flowing Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8157 PEEK, with CNT Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8167 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8169 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8173 PEEK, with PTFE Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8174 PEEK, with PTFE, lubricant modified Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8179 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8199 PEEK, with CNT Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8278/GY PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8317/RD PEEK, with glass fiber Polyetheretherketone, PEEK, Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Polyetheretherketone, PEEK, PTFE-Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing Polyetheretherketone, PEEK, Aramid Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8355 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8356 PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8432 PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8451 PEEK, with carbon fiber, lubricant modified Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8496 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8529 PEEK, with carbon fiber Polyetheretherketone, PEEK, Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified Polyaryletherketone (PAEK), Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 2205-7054 Blend based on polyaryl ether ketone, with glass fiber Polyaryletherketone (PAEK), Glass Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Polyaryletherketone (PAEK), Carbon Fiber Filled LUVOCOM®
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7994 PEEK, unreinforced Polyetheretherketone, PEEK, Unreinforced LUVOCOM®
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing Polyketone LUVOCOM®
Lehmann & Voss LUVOCOM® 1105/BK0873 PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Polyetheretherketone (PEEK) LUVOCOM®
Copyright © lookpolymers.com All Rights Reserved