Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : DSM Engineering Plastics > Category : Polyester, TP Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
DSM Arnite® AV2 340 PET-20% Glass Reinforced (European Grade) Polyethylene Terephthalate (PET), 20% Glass Reinforced Arnite®
DSM Arnite® AV2 370 /B PET-35% Glass Reinforced (European and Asian Grade) Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 370 XL-T PET-GF35 Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 390 PET-50% Glass Reinforced (European Grade) Polyethylene Terephthalate (PET), 50% Glass Reinforced Arnite®
DSM Arnite® AV2 390 XT PET GF50 Polyethylene Terephthalate (PET), 50% Glass Reinforced Arnite®
DSM Arnite® B427 SE/R PBT-GF35 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® B600SE PBT FR Polybutylene Terephthalate (PBT), Flame Retardant Arnite®
DSM Arnite® BM4 240 (PBT+PET)-MD20 PBT + PET, Mineral Filled Arnite®
DSM Arnite® T06 200 PBT (European and Asian Grade) Polybutylene Terephthalate (PBT), Unreinforced, Molded Arnite®
DSM Arnite® T08 200 (extrusion) PBT (European and Asian Grade) Polybutylene Terephthalate (PBT), Extrusion Grade Arnite®
DSM Arnite® TM4 440 (PBT+PET)-MD20 PBT + PET, Mineral Filled Arnite®
DSM Arnite® TV4 220 PBT-10% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled Arnite®
DSM Arnite® TV4 230 S PBT-GF15 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV4 240 S PBT-20% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV4 241 SN PBT-GF20 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 244 S PBT-GF20 FR Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 260 SN PBT-GF30 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 260 SXF PBT-GF30 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Arnite®
DSM Arnite® TV4 261 SF PBT-GF30 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® TV4 270 PBT-35% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled Arnite®
DSM Arnite® TV4 290 PBT-GF50 Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled Arnite®
DSM Arnite® TV4 441 (PBT+PET)-GF20 PBT + PET Blend, Glass Filled Arnite®
DSM Arnite® TV4 461 (PBT+PET)-GF30 PBT + PET Blend, Glass Filled Arnite®
DSM Arnite® TV4 461 KL (PBT+PET)-GF30 PBT + PET Blend, Glass Filled Arnite®
DSM Arnite® TV4 640 (PBT+PC) - GF20 Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV6 220 PBT-GF10 Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled Arnite®
DSM Arnite® TV6 240 PBT-GF20 Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV6 241 T Impact Modified PBT-20% Glass Reinforced (European Grade) Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV8 260 PBT-30% Glass Reinforced (European Grade) Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Arnite®
DSM Arnite® TZ4 254 S PBT-(GF+MD)25 FR(17) Polybutylene Terephthalate (PBT), Glass + Mineral Filled Arnite®
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 Polybutylene Terephthalate (PBT), Glass Bead Filled Arnite®
DSM Arnitel® EB463 41 Shore D, Blow Molding Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EL740-H/A Injection Molding; Other Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EM400-BP TPC-ET Polyester TPE Arnitel®
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EM630 63 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® EM631 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® EM631-HB TPC-ET Polyester TPE Arnitel®
DSM Arnitel® EM740 74 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PB420 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® PB420-B TPC-ET Polyester TPE Arnitel®
DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PB582-H Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL380 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL381-H TPC-ET Polyester TPE Arnitel®
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL420-H Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL461 Injection Molding Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL461 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL650 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PM460-H TPC-ET Polyester TPE Arnitel®
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® PM581 58 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® UM552 Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM Arnitel® VT3104 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® VT3108 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® XG5857 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® XG5858 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® XG6029 TPC-ET Polyester TPE Arnitel®
DSM Arnite® A02 307 PET Polyethylene Terephthalate (PET), Unreinforced Arnite®
DSM Arnite® A06 101 PET (European Grade) Polyethylene Terephthalate (PET), Unreinforced Arnite®
DSM Arnite® A06 300 PET (European Grade) Polyethylene Terephthalate (PET), Unreinforced Arnite®
DSM Arnite® A06 700 PET (European Grade) Polyethylene Terephthalate (PET), Unreinforced Arnite®
DSM Arnite® AV2 360 S PET-33% Glass Reinforced (European Grade) Polyethylene Terephthalate (PET), 30% Glass Reinforced Arnite®
DSM Arnite® AV2 365 SN PET-30% Glass Reinforced (European Grade) Polyethylene Terephthalate (PET), 30% Glass Reinforced Arnite®
DSM Arnite® AV2 370 HF PET-GF35 Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 370 XL PET-GF35 Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 370 XT PET-GF35 Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 372 PET-35% Glass Reinforced (European and Asian Grade) Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnite® AV2 390 XL PET GF50 Polyethylene Terephthalate (PET), 50% Glass Reinforced Arnite®
DSM Arnite® B434 SE PBT-GF20 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® B436 SE PBT-GF30 FR(17) Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant Arnite®
DSM Arnite® B600 SNF PBT FR Polybutylene Terephthalate (PBT), Flame Retardant Arnite®
Copyright © lookpolymers.com All Rights Reserved