DSM Arnitel® PM460-H TPC-ET

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnitel® PM460-H TPC-ET.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Injection Molding, Heat Stabilized
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ISO 1183
Melt Flow 9.6 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.6 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45

@Time 3.00 sec
45

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 19.5 MPa
2830 psi
ISO 527-1/-2
Tensile Stress 5.40 MPa

@Strain 5.00 %
783 psi

@Strain 5.00 %
ISO 527-1/-2
8.40 MPa

@Strain 10.0 %
1220 psi

@Strain 10.0 %
ISO 527-1/-2
13.3 MPa

@Strain 50.0 %
1930 psi

@Strain 50.0 %
ISO 527-1/-2
15.5 MPa

@Strain 100 %
2250 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 205 %
205 %
ISO 527-1/-2
Tensile Modulus 0.120 GPa
17.4 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °C
149 °F
ISO 75-1/-2