| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Arnite® AV2 390 XL PET GF50.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.78 g/cc | 0.0643 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Sim. To ISO 62 |
| Moisture Absorption | 0.120 % | 0.120 % | Sim. To ISO 62 |
| Viscosity | 20000 cP @Shear Rate 100000 1/s, Temperature 295 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 563 °F |
|
| 23000 cP @Shear Rate 100000 1/s, Temperature 315 °C |
23000 cP @Shear Rate 100000 1/s, Temperature 599 °F |
||
| 30000 cP @Shear Rate 100000 1/s, Temperature 270 °C |
30000 cP @Shear Rate 100000 1/s, Temperature 518 °F |
||
| 200000 cP @Shear Rate 1000 1/s, Temperature 295 °C |
200000 cP @Shear Rate 1000 1/s, Temperature 563 °F |
||
| 230000 cP @Shear Rate 1000 1/s, Temperature 315 °C |
230000 cP @Shear Rate 1000 1/s, Temperature 599 °F |
||
| 300000 cP @Shear Rate 1000 1/s, Temperature 270 °C |
300000 cP @Shear Rate 1000 1/s, Temperature 518 °F |
||
| Linear Mold Shrinkage, Flow | 0.0045 cm/cm | 0.0045 in/in | Sim. To ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | Sim. To ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 210 MPa | 30500 psi | ISO 527-1/-2 |
| Elongation at Break | 2.0 % | 2.0 % | ISO 527-1/-2 |
| Tensile Modulus | 19.0 GPa | 2760 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 6.50 J/cm² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| 6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature 23.0 °C |
4.28 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 20.0 µm/m-°C | 11.1 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 252 °C | 486 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 240 °C | 464 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.47 mm |
HB @Thickness 0.0579 in |
IEC 60695-11-10 |
| HB @Thickness 0.810 mm |
HB @Thickness 0.0319 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.5 @Frequency 1.00e+6 Hz |
3.5 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.8 @Frequency 100 Hz |
3.8 @Frequency 100 Hz |
IEC 60250 | |
| Dissipation Factor | 0.0020 @Frequency 100 Hz |
0.0020 @Frequency 100 Hz |
IEC 60250 |
| 0.011 @Frequency 1.00e+6 Hz |
0.011 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 250 V | 250 V | IEC 60112 |