| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Arnite® TV4 290 PBT-GF50.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.72 g/cc | 0.0621 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Sim. To ISO 62 |
| Moisture Absorption | 0.150 % | 0.150 % | Sim. To ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0025 cm/cm | 0.0025 in/in | Sim. To ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0095 cm/cm | 0.0095 in/in | Sim. To ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 145 MPa | 21000 psi | ISO 527-1/-2 |
| Elongation at Break | 1.8 % | 1.8 % | ISO 527-1/-2 |
| Tensile Modulus | 15.6 GPa | 2260 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 5.30 J/cm² @Temperature 23.0 °C |
25.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 1.15 J/cm² @Temperature 23.0 °C |
5.47 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
IEC 60695-11-10 |
| HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |