| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnitel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Arnitel® XG5857 TPC-ET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Water Absorption | 0.20 % | 0.20 % | Sim. To ISO 62 |
| Moisture Absorption | 0.650 % | 0.650 % | Sim. To ISO 62 |
| Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 88 @Time 3.00 sec |
88 @Time 0.000833 hour |
ISO 868 |
| Tensile Strength, Ultimate | 10.6 MPa | 1540 psi | ISO 527-1/-2 |
| Tensile Stress | 3.50 MPa @Strain 10.0 % |
508 psi @Strain 10.0 % |
ISO 527-1/-2 |
| 5.30 MPa @Strain 100 % |
769 psi @Strain 100 % |
ISO 527-1/-2 | |
| Elongation at Break | 440 % | 440 % | ISO 527-1/-2 |
| Tensile Modulus | 0.0600 GPa | 8.70 ksi | ISO 527-1/-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 195 °C | 383 °F | 10°C/min; ISO 11357-1/-3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 8.30e+12 ohm-cm | 8.30e+12 ohm-cm | IEC 60093 |
| Dielectric Strength | 19.8 kV/mm | 503 kV/in | IEC 60243-1 |