Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® A06 101 PET (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame retardant gradesEasy molding FR grades for connectorsToughened unfilled materials for durabilityHigh modulus, tight specification for critical auto componentsToughened reinforced resinsLow outgassing grades for reflector surfacesArnite extrusion resins: Specialized materials for specific usesPET for medical applicationsLoose buffer Optical fiber tubingPET for stock shapesApplicationsAutomotive:Connectors, sensors and E&E parts, Exterior fittings, Gear housings and motors, Brake valve bodiesElectrical & Electronic: Telecoms and IT connectors, Bobbins, Low voltage Power distribution, E-motor components, Lightings and Lamp fittingsConsumer Durables: Small AppliancesOther: Optical fiber tubingInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Humidity Absorption; Sim. to ISO 62
Melt Flow 8.04 g/10 min

@Load 2.16 kg,
Temperature 250 °C
8.04 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Calculated from Volume Flow Rate of 6 cm<sup>3</sup>/10min.; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 2.50 GPa
363 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.650 J/cm²

@Temperature 23.0 °C
3.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
10°C/min; ISO 11357-1/-3
UL RTI, Electrical 75.0 °C

@Thickness 0.930 mm
167 °F

@Thickness 0.0366 in
UL746B
75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.930 mm
167 °F

@Thickness 0.0366 in
UL746B
75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact 75.0 °C

@Thickness 0.930 mm
167 °F

@Thickness 0.0366 in
UL746B
75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL746B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
Oxygen Index 25 %
25 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
IEC 60093
Comparative Tracking Index >= 600 V
>= 600 V
PLC 0; UL 746A
Descriptive Properties Value Comments
Other Extrusion Yes
Profile extrusion Yes
Sheet extrusion Yes
Without Fillers Yes
Users viewing this material also viewed the following: