Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : DSM Engineering Plastics Product List

Category
Nylon 6, Glass Fiber Filled, Flame Retardant Nylon 66/Nylon 6 Blend, Glass Fiber Filled Nylon 66/6, 30% Glass Fiber Reinforced
Nylon 6, Unreinforced Film Nylon 6, Extruded
Nylon 6, Film Grade Nylon 6, 20% Glass Fiber Filled Nylon 6, Glass/Mineral Reinforced
Nylon 6, 30% Glass Fiber Filled Nylon 6, 30% Mineral Filled Nylon 6, Impact Grade
Nylon 6, 50% Glass Fiber Filled Nylon 6, 40% Glass Fiber Filled Nylon 6, Glass Filled, Impact Grade
Nylon 6, Unreinforced, Flame Retardant Nylon 6-3 Nylon 63, 35% Glass-Filled
Nylon 66, Unreinforced Nylon 66, 10% Glass Fiber Filled Nylon 66, 20% Glass Fiber Filled
Nylon 66, 30% Glass Fiber Filled Nylon 66, Glass/Mineral Filled Nylon 66, 40% Glass Fiber Filled
Nylon 66, 40% Mineral Filled Nylon 6, 60% Glass Fiber Filled Polyethylene Terephthalate (PET), 20% Glass Reinforced
Polyethylene Terephthalate (PET), 40% Glass Reinforced Polyethylene Terephthalate (PET), 50% Glass Reinforced Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Polybutylene Terephthalate (PBT), Flame Retardant PBT + PET, Mineral Filled Polybutylene Terephthalate (PBT), Extrusion Grade
Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled PBT + PET Blend, Glass Filled
Polybutylene Terephthalate (PBT), Glass + Mineral Filled Polybutylene Terephthalate (PBT), Glass Bead Filled Polyester TPE
Polyether Ester Elastomer High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight Renewable/Recycled Polymer
Nylon 46, Glass Fiber Reinforced Nylon 46, Flame Retarded + Glass Fiber Reinforced Nylon 46, Unreinforced
Nylon 46, Lubricated + Glass Fiber Reinforced Polyethylene Terephthalate (PET), Unreinforced Polyethylene Terephthalate (PET), 30% Glass Reinforced
Nylon 66, 30% Carbon Fiber Filled
Trade Name
Akulon® Akulon® Ultraflow™ Arnite®
Arnitel® Dyneema® EcoPaXX®
Novamid® Stanyl®
Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
DSM Akulon® F130-C PA6 Film Akulon®
DSM Akulon® F130-C2 PA6 Film Akulon®
DSM Akulon® F132-C1 PA6 Film Akulon®
DSM Akulon® F136 PA6 Film Akulon®
DSM Akulon® F136-E2 PA6 Film Akulon®
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Dry) Nylon 6, Unreinforced Akulon®
DSM Akulon® K222-KMV5 Nylon 6-25% Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K223-HM6 (BLACK) Nylon 6-30% Mineral Reinforced (European and Asian Grade) (Cond) Nylon 6, 30% Mineral Filled Akulon®
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) Nylon 6, 50% Glass Fiber Filled Akulon®
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-HG6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 30% Glass Fiber Filled Akulon®
DSM Akulon® K224-PG8 (Cond.) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Nylon 6, Glass Filled, Impact Grade Akulon®
DSM Akulon® S223-HG6 (Dry) 30% Glass Reinforced Nylon 66 (North America) Nylon 66, 30% Glass Fiber Filled Akulon®
DSM Akulon® S223-HG6 Nylon 66-30% Glass Reinforced (European and Asian Grade) (Cond) Nylon 66, 30% Glass Fiber Filled Akulon®
DSM Akulon® Ultraflow K-FPG8 PA6-I-GF40 Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Akulon® Ultraflow™ K-FHG6 Nylon 6-30% Glass Reinforced (European Grade) (Cond) Nylon 6, 30% Glass Fiber Filled Akulon® Ultraflow™
DSM Arnite® B600SE PBT FR Polybutylene Terephthalate (PBT), Flame Retardant Arnite®
DSM Arnite® TV4 240 PBT-20% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled Arnite®
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Arnite®
DSM Arnite® TV4 441 (PBT+PET)-GF20 PBT + PET Blend, Glass Filled Arnite®
DSM Arnite® TZ6 280 BLK (NCP-4718/B) PBT-(GF+GB)40 Polybutylene Terephthalate (PBT), Glass Bead Filled Arnite®
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL420-H Injection Molding Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM EcoPaXX® Q-PG6 PA410-I-GF30 Renewable/Recycled Polymer EcoPaXX®
DSM EcoPaXX® Q-X07207 PA410-I Renewable/Recycled Polymer EcoPaXX®
DSM Novamid® 1010G30 NA PA6-GF30 Nylon 6, 30% Glass Fiber Filled Novamid®
DSM Novamid® 1010GN2-15 NAT PA6-GF15 FR(17) Nylon 6, Glass/Mineral Reinforced Novamid®
DSM Novamid® 1013C5 PA6 Nylon 6, Unreinforced Novamid®
DSM Novamid® 1017GH33 BK701 PA6-GF33 Nylon 6, 30% Glass Fiber Filled Novamid®
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Nylon 46, Glass Fiber Reinforced Stanyl®
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Cond) Nylon 46 Stanyl®
DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Nylon 46, Glass Fiber Reinforced Stanyl®
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Nylon 46, Glass Fiber Reinforced Stanyl®
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Nylon 46, Glass Fiber Reinforced Stanyl®
DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America) Nylon 46, Unreinforced Stanyl®
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond) Nylon 46, Unreinforced Stanyl®
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Nylon 46, Unreinforced Stanyl®
DSM Akulon® K224-G3 Nylon 6-15% Glass Reinforced (European and Asian Grade) (Dry) Nylon 6, 20% Glass Fiber Filled Akulon®
DSM Akulon® S223-DK Nylon 66 (European Grade) (Dry) Nylon 66, Unreinforced Akulon®
DSM Arnite® AV2 370 XL PET-GF35 Polyethylene Terephthalate (PET), 40% Glass Reinforced Arnite®
DSM Arnitel® EL250 TPC-ET Polyester TPE Arnitel®
DSM Arnitel® UM551-V Polyether Ester Elastomer (European Grade) Polyether Ester Elastomer Arnitel®
DSM EcoPaXX® Q-KGS6 PA410-GF30 FR Renewable/Recycled Polymer EcoPaXX®
DSM Akulon® K223-P2 Impact Modified Nylon 6 (European Grade) (Cond) Nylon 6, Impact Grade Akulon®
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Dry) Nylon 6, 40% Glass Fiber Filled Akulon®
DSM Arnite® TV6 260 T PBT-I-GF30 Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled Arnite®
DSM Arnitel® UM551 55 Shore D Copolyester Elastomer (North America) Polyester TPE Arnitel®
DSM Stanyl® TW241F5 PA46-GF25 Nylon 46, Glass Fiber Reinforced Stanyl®
Copyright © lookpolymers.com All Rights Reserved