| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Arnite® B600 SNF PBT FR.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
| Water Absorption | 0.40 % | 0.40 % | Sim. To ISO 62 |
| Moisture Absorption | 0.200 % | 0.200 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 45.0 MPa | 6530 psi | ISO 527-1/-2 |
| Elongation at Yield | 3.0 % | 3.0 % | ISO 527-1/-2 |
| Tensile Modulus | 2.30 GPa | 334 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C | 293 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
IEC 60695-11-10 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.2 @Frequency 1.00e+6 Hz |
3.2 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.4 @Frequency 100 Hz |
3.4 @Frequency 100 Hz |
IEC 60250 | |
| Dissipation Factor | 0.0030 @Frequency 100 Hz |
0.0030 @Frequency 100 Hz |
IEC 60250 |
| 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
IEC 60250 |