Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer DSM Engineering Plastics
Trade Name Arnitel®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.Characteristics of Arnitel:Excellent strength over a wide range of temperaturesExcellent dynamic properties e.g. creep and fatigueHigh heat resistanceExceptional resistance to oils and greasesGood chemical resistanceHigh degree of versatility in processingEasy coloring using masterbatchesSurface quality from high gloss to texturedExcellent heat resistance (long term 165°C)Good electrical insulation propertiesLow moisture absorption, excellent dimensional stabilityEasy flow, fast cooling timesTypical Applications: Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in consumer electronic companies. Arnitel® is a good choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.Information provided by DSM.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Melt Flow 3.69 g/10 min
<br>@Load 10.0 kg,<br> Temperature 230 °C
3.69 g/10 min
<br>@Load 22.0 lb,<br> Temperature 446 °F
Calculated from Volume Flow Rate of 3 cm&lt;sup&gt;3&lt;/sup&gt;/10 min; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
3 s; ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527-1/-2
Tensile Strength, Yield 11.3 MPa
<br>@Strain 5.00 %
1640 psi
<br>@Strain 5.00 %
ISO 527-1/-2
16.5 MPa
<br>@Strain 10.0 %
2390 psi
<br>@Strain 10.0 %
ISO 527-1/-2
22.3 MPa
<br>@Strain 50.0 %
3230 psi
<br>@Strain 50.0 %
ISO 527-1/-2
26.7 MPa
<br>@Strain 100 %
3870 psi
<br>@Strain 100 %
ISO 527-1/-2
Elongation at Break 150 %
150 %
ISO 527-1/-2
Tensile Modulus 0.300 GPa
43.5 ksi
ISO 527-1/-2
Izod Impact, Notched (ISO) NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched 1.40 J/cm²
<br>@Temperature -30.0 °C
6.66 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75-1/-2
Vicat Softening Point 105 °C
221 °F
50°C/h 50N; ISO 306
205 °C
401 °F
50°C/h 10N; ISO 306
Descriptive Properties Value Comments
Blow Molding Yes
Heat stabilized or stable to heat Yes
High impact or impact modified Yes
Without Fillers Yes
Copyright © lookpolymers.com All Rights Reserved