| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Arnite® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Arnite® TV4 261 SF PBT-GF30 FR(17).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.65 g/cc | 0.0596 lb/in³ | ISO 1183 |
| Water Absorption | 0.30 % | 0.30 % | Sim. To ISO 62 |
| Moisture Absorption | 0.150 % | 0.150 % | Sim. To ISO 62 |
| Viscosity | 9000 cP @Shear Rate 100000 1/s, Temperature 270 °C |
9000 cP @Shear Rate 100000 1/s, Temperature 518 °F |
|
| 10000 cP @Shear Rate 100000 1/s, Temperature 250 °C |
10000 cP @Shear Rate 100000 1/s, Temperature 482 °F |
||
| 20000 cP @Shear Rate 100000 1/s, Temperature 230 °C |
20000 cP @Shear Rate 100000 1/s, Temperature 446 °F |
||
| 1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 270 °C |
1.00e+6 cP @Shear Rate 1.00 1/s, Temperature 518 °F |
||
| 2.00e+6 cP @Shear Rate 1.00 1/s, Temperature 250 °C |
2.00e+6 cP @Shear Rate 1.00 1/s, Temperature 482 °F |
||
| 3.50e+6 cP @Shear Rate 1.00 1/s, Temperature 230 °C |
3.50e+6 cP @Shear Rate 1.00 1/s, Temperature 446 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 130 MPa | 18900 psi | ISO 527-1/-2 |
| Elongation at Break | 2.5 % | 2.5 % | ISO 527-1/-2 |
| Tensile Modulus | 11.0 GPa | 1600 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 5.00 J/cm² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
| 5.00 J/cm² @Temperature -30.0 °C |
23.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ISO 75-1/-2 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
IEC 60695-11-10 |
| V-0 @Thickness 0.750 mm |
V-0 @Thickness 0.0295 in |
IEC 60695-11-10 | |
| Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| 960 °C @Thickness 0.750 mm |
1760 °F @Thickness 0.0295 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 4.0 @Frequency 100 Hz |
4.0 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 28.0 kV/mm | 711 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.0025 @Frequency 100 Hz |
0.0025 @Frequency 100 Hz |
IEC 60250 |
| 0.014 @Frequency 1.00e+6 Hz |
0.014 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 300 V | 300 V | IEC 60112 |