Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON SD000 PA12 LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP KZ002 Acetal LNP* THERMOCOMP* KZ002 is a compound based on Acetal containing 10% Milled Glass. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66 LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp WX01910L PBT LNP* Thermocomp* WX01910L is a compound based on Thermoplastic Polyester containing Proprietary Fillers. Characteristics of this grade are: Low Extractable.This data was supplied by SABIC-IP for t.. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.040 cm/cm @Time 86400 sec |
0.010 - 0.040 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 LNP THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.040 cm/cm @Time 86400 sec |
0.020 - 0.040 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |