Material Notes:
FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyethylene specially developed for the manufacture of pressure pipes and fittings. Its well balanced property profile and composition makes FINATHENE® 3802 Blue perfectly suited for potable water distribution.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.941 g/cc
0.0340 lb/in³
ASTM D 792
Viscosity 1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 190 °C
1.30e+6 cP

@Shear Rate 100 1/s,
Temperature 374 °F
ATOFINA research test
Environmental Stress Crack Resistance >= 700 hour
>= 700 hour
ASTM D1693
Oxidative Induction Time (OIT) >= 20 min
>= 20 min
210°C; EN 728
>= 30 min
>= 30 min
200°C; EN 728
Melt Flow 0.20 g/10 min

@Load 2.16 kg
0.20 g/10 min

@Load 4.76 lb
ASTM D 1238
0.92 g/10 min

@Load 5.00 kg
0.92 g/10 min

@Load 11.0 lb
ASTM D 1238
High Load Melt Index 18 g/10 min

@Load 21.6 kg
18 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 MPa
4640 psi
ISO 527
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO R527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Modulus of Elasticity 0.700 GPa
102 ksi
ISO 178
Flexural Modulus 0.700 GPa
102 ksi
ASTM D 790
Charpy Impact, Notched >= 1.00 J/cm²

@Temperature 23.0 °C
>= 4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 170
Thermal Properties Metric English Comments
Heat of Fusion 161 J/g
69.3 BTU/lb
DSC
CTE, linear 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 2.00 J/g-°C
0.478 BTU/lb-°F
DSC
2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
DIN 52612
0.200 W/m-K

@Temperature 150 °C
1.39 BTU-in/hr-ft²-°F

@Temperature 302 °F
DIN 52612
Melting Point 125 - 129 °C
257 - 264 °F
crystalline; DSC
Vicat Softening Point 125 °C
257 °F
ISO 306
Brittleness Temperature -100 °C
-148 °F
ASTM D 746
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
IEC 93
Surface Resistance >= 1.00e+16 ohm
>= 1.00e+16 ohm
IEC 93
Dielectric Constant 2.45

@Frequency 1000 Hz
2.45

@Frequency 1000 Hz
IEC 250
Dielectric Strength 16.0 kV/mm
406 kV/in
IEC 243
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
IEC 250
Users viewing this material also viewed the following: