Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 161 J/g | 69.3 BTU/lb | DSC |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |