Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 18 g/10 min @Load 21.6 kg, Temperature 240 °C |
18 g/10 min @Load 47.6 lb, Temperature 464 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PC/ABS 1420 PRE-ELEC PC/ABS 1420 is a conductive thermoplastic compound based on a PC/ABS blend. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PR.. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg, Temperature 200 °C |
18 g/10 min @Load 47.6 lb, Temperature 392 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg, Temperature 190 °C |
18 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE105B WHITE MASTERBATCH WHITE PE105B is a white low density polyethylene based masterbatch highly-concentrated with TiO2 without any addition of filler and fluorescence whitener. This product is designed for film applicati.. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg, Temperature 190 °C |
18 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE650 GREEN MASTERBATCH GREEN PE650 is a green LDPE based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Green 7.Method of Usage: GREEN PE 650 is designed for .. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg |
18 g/10 min @Load 47.6 lb |
ISO 1133 |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg |
18 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg |
18 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
High Load Melt Index | 18 g/10 min @Load 21.6 kg |
18 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Lacqtene® 2001 TBK 40 HDPE pipe
(discontinued **) LACQTENE® 2002 TBK 40 is a medium density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2002 TBK 40 is a black compound especially developed for.. |