Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.92 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.92 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |
|||
Melt Flow | 0.92 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.92 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC) TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo.. |
|||
Melt Flow | 0.92 g/10 min @Load 5.00 kg |
0.92 g/10 min @Load 11.0 lb |
ISO 1133 |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Melt Flow | 0.92 g/10 min @Load 5.00 kg |
0.92 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Melt Flow | 0.92 g/10 min @Load 5.00 kg |
0.92 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |