ExxonMobil Escorene® UL 7840E Adhesive Application Resin

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® UL 7840E Adhesive Application Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra UL 7840E is a 31.4% vinyl acetate copolymer that has good compatibility with both hydrocarbon and natural tackifiers and is suitable for making hot melt adhesives adn sealants. UL 7840E contains an additive package to improve pellet flowability an handling. Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsHot Melt AdhesivesIndustrial Sealants Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ExxonMobil Method
Vinyl Acetate Content 31.4 %
31.4 %
ExxonMobil Method
Melt Flow 43.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
15s; ASTM D2240
Tensile Strength at Break 3.03 MPa
440 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.0124 GPa
1.80 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 57.8 °C
136 °F
Peak Melting Temperature; ExxonMobil Method