Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Solvay Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins. This resin also offer high deflection temperatures and outstanding resistance to environmental stress cracking. Radel® polymers are inherently flame retardant, provide excellent thermal stability and possess good electrical properties.Features: Acid Resistant; Autoclave Sterilizable; Base Resistant; Biocompatible; Detergent Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Flame Retardant; General Purpose; Good Chemical Resistance; Good Dimensional Stability; Good Electrical Properties; Good Sterilizability; Good Thermal Aging Resistance; Good Thermal Stability; Heat Sterilizable; High ESCR (Stress Crack Resist.); High Heat Resistance; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable; Ultra High ToughnessUses: Automotive Applications; Dental Applications; Food Service Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Membranes; Surgical InstrumentsAdditional Properties: Steam Sterilization - > 1000 CyclesAutomotive Specifications ASTM D6394 SP0312Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.37 %

@Time 86400 sec
0.37 %

@Time 24.0 hour
ISO 62
Water Absorption at Saturation 1.1 %
1.1 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Thickness 3.18 mm
0.0070 in/in

@Thickness 0.125 in
Melt Flow 14 - 20 g/10 min

@Load 5.00 kg,
Temperature 365 °C
14 - 20 g/10 min

@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 69.6 MPa

@Thickness 3.18 mm
10100 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break 60 - 120 %

@Thickness 3.18 mm
60 - 120 %

@Thickness 0.125 in
ASTM D638
Elongation at Yield 7.2 %

@Thickness 3.18 mm
7.2 %

@Thickness 0.125 in
ASTM D638
Tensile Modulus 2.34 GPa

@Thickness 3.18 mm
339 ksi

@Thickness 0.125 in
ASTM D638
Flexural Strength 91.0 MPa

@Strain 5.00 %,
Thickness 3.18 mm
13200 psi

@Strain 5.00 %,
Thickness 0.125 in
ASTM D790
Flexural Modulus 2.41 GPa

@Thickness 3.18 mm
350 ksi

@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 399 kJ/m²

@Thickness 3.18 mm
190 ft-lb/in²

@Thickness 0.125 in
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Deflection Temperature at 1.8 MPa (264 psi) 207 °C

@Thickness 3.20 mm
405 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Flammability, UL94 V-0

@Thickness 0.762 mm
V-0

@Thickness 0.0300 in
Optical Properties Metric English Comments
Refractive Index 1.672
1.672
ASTM D542
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+15 ohm-cm
9.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.44

@Frequency 60.0 Hz
3.44

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm

@Thickness 3.18 mm
381 kV/in

@Thickness 0.125 in
ASTM D149
>= 200 kV/mm

@Thickness 0.0254 mm
>= 5080 kV/in

@Thickness 0.00100 in
ASTM D149
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 51; NSF 61
Processing Properties Metric English Comments
Zone 1 338 - 388 °C
640 - 730 °F
Zone 2 338 - 388 °C
640 - 730 °F
Zone 3 338 - 388 °C
640 - 730 °F
Zone 4 338 - 388 °C
640 - 730 °F
Zone 5 338 - 388 °C
640 - 730 °F
Adapter Temperature 327 - 371 °C
621 - 700 °F
Melt Temperature 360 - 391 °C
680 - 736 °F
Mold Temperature 138 - 163 °C
280 - 325 °F
Die Cooling Temperature 327 - 371 °C
621 - 700 °F
Drying Temperature 149 °C
300 °F
171 °C

@Time 14400 sec
340 °F

@Time 4.00 hour
Descriptive Properties Value Comments
Agency Ratings FAA FAR 25.853a; ISO 10993
Availability Asia Pacific
Europe
Latin America
North America
Color Clear/Transparent
Form Pellets
Processing Technique Blow Molding; Extrusion; Film Extrusion
Injection Molding; Machining
Profile Extrusion; Sheet Extrusion; Thermoforming
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.2:1.0