Polymer Property : CTE, linear, Parallel to Flow = 31.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP COLORCOMP G1000 PSU
LNP* COLORCOMP* G1000 is an unfilled Polysulfone resin. Added feature of this grade is: Transparent.
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate or ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**)
Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)  (discontinued **)
Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)  (Unverified Data**)
Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)  (discontinued **)
Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® P-1835 Polysulfone (PSU)  (discontinued **)
Udel P-1835 polysulfone is a powdered grade well suited for the fabrication of porous membranes. The membranes can be made into hollow fibers, tubes, plates, or spiral wound elements. They are used ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Solvay Specialty Polymers Udel® M-2300 MR Polysulfone (PSU), Mold Release  (discontinued **)
Udel M-2300 MR is an injection-moldable, low-color grade of polysulfone that is nearly water white in color. This material contains a mold release which aids part ejection when parts with low draft ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose
Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ N1006A-M41 Nylon
Impact modified unreinforced injection grade. Main Features:High elongationHigh impact strengthExamples of applications are:Retainers for quick connectorFlexible band
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 100 °C
31.1 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP
SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID..
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU)
Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Ajedium™ Films -- Udel® PSU P-1700 NT-11 Polysulfone (PSU)
Udel® P-1700 polysulfones are tough, high-strength thermoplastics that are suitable for continuous use up to 300°F (149°C). Udel Film is resistant to oxidation and hydrolysis and withstand ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Ajedium™ Films -- Veradel® PES 201 NT Polyethersulfone (PESU)
Veradel® PES 201 NT polyethersulfone is a tough, high-strength thermoplastics that are suitable for continuous use up to 356°F (180°C). Veradel® film is resistant to oxidation and hydrol..
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC
LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare.
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Thickness 3.18 mm
31.1 µin/in-°F

@Thickness 0.125 in
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Udel® P-1700 LCD Polysulfone (PSU)
Udel® P-1700 LCD polysulfone is especially well suited for the fabrication of porous membranes for filtration applications. The membranes are usually in the form of hollow fibers, but tube, plate..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion..
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)
Udel® P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved ..
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS
LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber.
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
31.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp FF004 PE
LNP THERMOCOMP* FF004 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East)
XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 577 BK000 Acetal (POM)  (Unverified Data**)
20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler with high stiffness low warpage and low creep for sup..