Density 1.29 g/cc
0.0466 lb/in³
ISO 1183-1
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DL003 is a compound based on Polycarbonate resin containing PTFE.
Density 1.29 - 1.49 g/cc

@Temperature 250 - 250 °C
0.0466 - 0.0538 lb/in³

@Temperature 482 - 482 °F
Average value: 1.40 g/cc Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Density 1.29 - 1.70 g/cc
0.0466 - 0.0614 lb/in³
Average value: 1.53 g/cc Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Density 1.29 - 1.61 g/cc
0.0466 - 0.0582 lb/in³
Average value: 1.46 g/cc Grade Count:65
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Density 1.29 g/cc
0.0466 lb/in³
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating
LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozo..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Lucobit Lucobatch® 1850 T100 Polyolefin TPO Granules
Lucobatch® 1850 T100 is a highly stabilized polyolefin based TPO granules. Lucobatch® 1850 T100 is employed as a master batch. Blended with suitable polyolefins, tunnel membranes are built of ..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific)
LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS
LNP* STAT-KON* AX06518 is a compound based on ABS resin containing Stainless Steel. Added features of this material include: Electrically Conductive, Flame Retardant, EMI/RFI Shielding.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Solvay Specialty Polymers AvaSpire® AV-651 Polyaryletherketone (PAEK)
AvaSpire® AV-651 is an unreinforced polyaryletherketone (PAEK) that offers more ductility and impact strength than PEEK, with higher chemical and environmental stress cracking resistance than Ava..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Techmer ES Electrablend® PPS 06001
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DE002 PC
LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DE0029 PC
LNP* STAT-KON* DE0029 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP STAT-KON DEL13PXC PC (Europe-Africa-Middle East)
LNP* Stat-kon* DEL13PXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Superior Molding.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66
LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000/51 GV 30 HWCP 30% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperature..
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1184
Fainplast Compounds KL 94 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
Density 1.29 g/cc
0.0466 lb/in³
A. Schulman ComAlloy Lubrilon® 637 Nylon 6/6, Carbon Fiber/Molybdenum Disulfide Filled
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Density 1.29 g/cc
0.0466 lb/in³
(DAM); ISO 1183
DSM Stanyl® TW200F3 (COND) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
DSM Stanyl® TW200F3 (DAM) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12
LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System.