Polymer Property : Melt Temperature = 680 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 360 - 399 °C
680 - 750 °F
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Melt Temperature 360 - 393 °C
680 - 739 °F
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU)
Information provided by PolyOne
Melt Temperature 360 - 404 °C
680 - 759 °F
Average value: 374 °C Grade Count:6
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Melt Temperature 360 - 366 °C
680 - 691 °F
LNP Lubricomp® EFL-4034 LE BK8-065 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **
Features: Low Extractables, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g..
Melt Temperature 360 - 366 °C
680 - 691 °F
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Melt Temperature 360 - 366 °C
680 - 691 °F
LNP Stat-Kon® PDX-E-99550 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
Melt Temperature 360 - 366 °C
680 - 691 °F
LNP Stat-Kon® PDX-E-99689 CCS Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued..
Melt Temperature 360 - 366 °C
680 - 691 °F
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement  (discontinued **)
Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st..
Melt Temperature 360 - 382 °C
680 - 720 °F
Molding
PolyOne Edgetek® PF-40GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 360 - 375 °C
680 - 707 °F
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced  (Unverified Data**)
High flow, High Heat resistance, Low Warpage, for Thick Walled (>0.2mm) or thin (
Melt Temperature 360 - 390 °C
680 - 734 °F
LATI Larpeek 50 PEEK
Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;..
Melt Temperature 360 - 390 °C
680 - 734 °F
LATI Latiohm 88/10-06 CNT PEEK
Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided..
Melt Temperature 360 - 391 °C
680 - 736 °F
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
Melt Temperature 360 - 391 °C
680 - 736 °F
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Melt Temperature 360 - 391 °C
680 - 736 °F
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
Melt Temperature 360 - 391 °C
680 - 735 °F
RTP Company RTP 2000 R-4300 Polyphenylsulfone Alloy
Melt Temperature 360 - 399 °C
680 - 750 °F
RTP Company RTP 2299 X 133087 A EG Polyetheretherketone (PEEK), Carbon Nanotube - Static Dissipative - Extrusion Grade
Preliminary Data Sheet
Melt Temperature 360 - 370 °C
680 - 698 °F
Celanese ZENITE 7145L LCP, 45% Glass Reinforced
Zenite« 7145L is a 45% glass fiber reinforced and lubricated liquid crystal polymer for injection molding. It has excellent impact resistance and high heat deflection temperature.Information provid..
Melt Temperature 360 - 370 °C
680 - 698 °F
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced
Zenite 7244 is a 40% glasslmineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese
Melt Temperature 360 °C
680 °F
Optimal
BASF Ultrason® E 2010 MR SW 10111 PESU
Description: Unreinforced, medium viscosity standard injection molding grade, demolding optimized. Abbreviated designation according to ISO 1043-1: PESU.Information provided by BASF
Melt Temperature 360 - 370 °C
680 - 698 °F
Celanese ZENITE 17311 EFT LCP, 35% Mineral / Glass Reinforced
ZENITE« 17311 EFT is a 35% glass and mineral reinforced grade. This grade offers excellent flowability, low warpage, excellent surface appearance, and excellent dimensional stability. Application f..
Melt Temperature 360 - 399 °C
680 - 750 °F
Molding
PolyOne Edgetek® PI-20GF/000 Polyetherimide (PEI), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 360 - 390 °C
680 - 734 °F
LATI Latilub 88/50-20T PEEK, PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter..
Melt Temperature 360 - 370 °C
680 - 698 °F
E-Polymers SEPAZ® C245GP 45% Glass Fiber Reinforced LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..
Melt Temperature 360 - 388 °C
680 - 730 °F
Molding
PolyOne Edgetek® PI-20CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 360 - 388 °C
680 - 730 °F
Molding
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 360 - 391 °C
680 - 735 °F
RTP Company RTP 2000 R-4400 Polyphenylsulfone Alloy
Melt Temperature 360 - 390 °C
680 - 734 °F
LATI Latilub 88/50-30GRT PEEK, Graphite/PTFE Filled
Self-lubricating product based on Polyetheretherketone (PEEK). Graphite / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Melt Temperature 360 - 399 °C
680 - 750 °F
RTP Company RTP 2299 X 120337 Polyetheretherketone (PEEK), Carbon Fiber - Wear Resistant
Melt Temperature 360 - 375 °C
680 - 707 °F
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced
Super High Flow, High heat Resistance and Low Warp for Thin Parts.Information provided by Celanese