Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics Cycoloy® MC5215 PC+ABS
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated F..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant
Information provided by Polykemi AB
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East)
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Manifattura Cattaneo PA 6.6 30% GF Nylon, Glass Filled
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Density 1.29 g/cc
0.0466 lb/in³
DIN EN ISO 1183-1
Kraiburg TPE COPEC® CC7OCN Thermoplastic Elastomer, adhesion to ABS, PC and PC/ABS
The VS/AD1 Series is recommended for applications in the consumer electronics section. The compounds feature an exceptionally silky and velvety surface, accompanied by excellent adhesion properties ..
Density 1.29 g/cc
0.0466 lb/in³
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating
LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozo..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC
LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON AX06518 ABS (Asia Pacific)
LNP* Stat-kon* AX06518 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, Fl..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DE002 PC
LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon DEF13 PC
LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Stat-kon DEP32XXC PC (Asia Pacific)
LNP* STAT-KON* DEP32XXC is a compound based on Polycarbonate resin containing PTFE, Silicone, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied b..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific)
Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific)
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East)
Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable ..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6000 GV 20 HWCP 20% Glass Fiber Nylon 6, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
CP-Polymer-Technik Wellamid® 6600/50 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until 0°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Density 1.29 g/cc
0.0466 lb/in³
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
E-Polymers TEKAMID® TB120GM20 , 20% GF/MF Reinforced PA6, DAM
20% GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd.
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Adell AR-34 Nylon 66, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Density 1.29 g/cc
0.0466 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re..
Density 1.29 g/cc
0.0466 lb/in³
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Albis Plastics ASA 02A MR20 , 20% Mineral Filled  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..
Density 1.29 g/cc
0.0466 lb/in³
A. Schulman ComAlloy Hiloy® 716 PPS, Carbon Fiber Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East)
NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C.