Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 220 °C | 428 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and .. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM D3418 |
Quadrant EPP Quadrant PPSU LSG PPSU, Extruded, Unfilled, Polyphenylsulfone (ASTM Product Data Sheet) |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be g.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | |
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersin.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU) Veradel® A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excelle.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU) Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propert.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Vira.. |
|||
Glass Transition Temp, Tg | 220 - 225 °C | 428 - 437 °F | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | Postcured, Dry |
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ISO 11357-1/-2 |
BASF Ultrason® P 3010 MR SW 10101 PPSU Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | DSC |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | DSC |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU)
(Unverified Data**) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing .. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | ASTM E1356 |
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | DSC |
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU)
(Unverified Data**)&l Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propertie.. |
|||
Glass Transition Temp, Tg | 220 °C | 428 °F | DSC |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |