Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 6.90 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
12.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS
Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance.
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific)
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.
Izod Impact, Notched 6.90 J/cm

@Temperature -10.0 °C
12.9 ft-lb/in

@Temperature 14.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific)
19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only
Izod Impact, Notched 6.90 J/cm

@Temperature -10.0 °C
12.9 ft-lb/in

@Temperature 14.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East)
19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
12.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)  (Unverified Data**)
Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar..
Izod Impact, Notched 6.90 J/cm

@Temperature -10.0 °C
12.9 ft-lb/in

@Temperature 14.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer
19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only
Izod Impact, Notched 6.90 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
Kotec Carbotex K-20MRA30 Polycarbonate, General Purpose, Mold Release Grade
Features: Mold release, Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesIn..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade
UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
Kotec Carbotex K-20UVR30 Polycarbonate, General Purpose, UV Stability + Mold Release Grade
Features: UV stability, Mold release Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household ap..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
12.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
notch
Kraton® G1650 + PP blend (20/80)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Haysite Thermalate® H330 Glass Mat Reinforced Polyester Laminate
Platen Insulation. A thermoset insulation material with exceptional property retention at operating temperatures up to 550 F. Demonstrating superior compressive strength at high temperature, this g..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU)
Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC
LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added featu..
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC
LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256; ISO 180/4A
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Resin
Overview: CALIBREâ„¢ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi..
Izod Impact, Notched 6.90 J/cm

@Temperature 23.0 °C
12.9 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin
Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.20 mm
12.9 ft-lb/in

@Thickness 0.126 in
ASTM D256
Covestro Bayblend® T 85 Polycarbonate/ABS Blend
High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 ..
Izod Impact, Notched 6.90 J/cm

@Thickness 3.17 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Izod Impact, Notched 6.90 J/cm
12.9 ft-lb/in
ASTM D256
ABW Polymers PC/PET Alloy
Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles..