Thermal Properties Metric English Comments
Glass Transition Temp, Tg 220 °C
428 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg
The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and ..
Glass Transition Temp, Tg 220 °C
428 °F
DSC, 20°C/min.; ISO 11357-1/-2
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data)
Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be g..
Glass Transition Temp, Tg 220 °C
428 °F
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi..
Glass Transition Temp, Tg 220 °C
428 °F
Cookson Group Plaskon® SMT-B-1FX (146.801) Epoxy Molding Compound for PBGAs  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It is a reduced catalyst version of SMT-B-1F and provide..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU)
Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU ..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU)
Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU)
Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU)
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU)
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)
Veradel® PESU was formerly marketed as Gafone™ PESU. Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They ca..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
Veradel® A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles.PESU offers excellen..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU)
Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propert..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU)
Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Vira..
Glass Transition Temp, Tg >= 220 °C
>= 428 °F
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System
Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea..
Glass Transition Temp, Tg >= 220 °C
>= 428 °F
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System
Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr..
Glass Transition Temp, Tg 220 °C
428 °F
Postcured, Dry
Hexcel® HexTOOL™ M81 Multi-Axial High Temperature Epoxy Tooling Compound
HexTOOL™ M81 Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequ..
Glass Transition Temp, Tg 220 °C
428 °F
ISO 11357-1/-2
BASF Ultrason® P 3010 MR SW 10101 PPSU
Description: Unreinforced, higher viscosity injection molding grade, flame retardant and with improved chemical resistance. This grade is black colored and demolding optimized. Abbreviated designati..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t..
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t..
Glass Transition Temp, Tg 220 °C
428 °F
DSC
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)  (Unverified Data**)
Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par..
Copyright © lookpolymers.com All Rights Reserved