Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 399 kJ/m² @Thickness 3.18 mm |
190 ft-lb/in² @Thickness 0.125 in |
ASTM D1822 |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Tensile Impact Strength | 399 kJ/m² | 190 ft-lb/in² | ASTM D1822 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Tensile Impact Strength | 399 kJ/m² @Thickness 3.18 mm |
190 ft-lb/in² @Thickness 0.125 in |
ASTM D1822 |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Tensile Impact Strength | 399 kJ/m² @Thickness 3.18 mm |
190 ft-lb/in² @Thickness 0.125 in |
ASTM D1822 |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Tensile Impact Strength | 399 kJ/m² @Thickness 3.18 mm |
190 ft-lb/in² @Thickness 0.125 in |
ASTM D1822 |
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Tensile Impact Strength | 399 kJ/m² | 190 ft-lb/in² | ASTM D1822 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Tensile Impact Strength | 399 kJ/m² | 190 ft-lb/in² | ASTM D1822 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Tensile Impact Strength | 400 kJ/m² | 190 ft-lb/in² | At -20°C; ASTM D1822 |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 400 kJ/m² | 190 ft-lb/in² | At 23°C; ASTM D1822 |
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Impact Strength | 399 kJ/m² | 190 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE HYA021L High Density Polyethylene Resin Product Description: HYA021L is a molecular weight, high-density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: Latin A.. |
|||
Tensile Impact Strength | 399 kJ/m² @Temperature -40.0 °C |
190 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil Paxon™ BA53-035 Blow Molding Resin
(discontinued **) BA53-035 is a high molecular weight, high density polyethylene copolymer offering an outstanding combination of stiffness and toughness. The resin provides superior melt strength and impact resista.. |