Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 138 - 163 °C | 280 - 325 °F | |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Mold Temperature | 138 - 163 °C | 280 - 325 °F | |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Mold Temperature | 138 - 163 °C | 280 - 325 °F | |
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified) Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1605 Low Shrink, Medium Strength BMC 1605 is an excellent low-cost HB material with low shrink and medium strength. Has excellent surface finish and gloss. Can be injection, compression or transfer molded. UL® recognized. This mat.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 350 Thermoset Polyester, Medium Impact BMC 350 is a cosmetic and appliance grade material with excellent heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical ap.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5209 Mineral Filled, Glass Reinforced Polyester BMC 5209 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resis.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620X molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil .. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 800 Thermoset Polyester, Corrosion Resistant BMC 800 compounds are UL rated 94V0/5V. These compounds exhibit excellent strength, corrosion and weather resistant properties. As with all other BMCI compounds, this Series can be supplied in logs,.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 880 Medium Strength Molding Compound BMC 880 is a medium strength, low shrink molding compound designed for outdoor applications. This material is UL Listed 94-V0/5V and is UL approved for outdoor use. It can be supplied in bulk or ext.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 902 Thermoset Polyester, Soft Flow Encapsulation Grade BMC 902 is a medium strength, high flow molding compound that meets Ford Specification ESFM3D114- A. BMC 902 has excellent electrical properties and creep resistance. It can be pigmented in a wide r.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade BMC 400 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, and power tool housings. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 5338 Mineral Filled, Glass Reinforced Polyester BMC 5338 molding compound is a mineral Filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ex.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Mold Temperature | 138 - 166 °C | 280 - 330 °F | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |