Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16 - 20 g/10 min | 16 - 20 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP6025 PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Melt Flow | 16 - 20 g/10 min | 16 - 20 g/10 min | ASTM D1238 |
S&E Specialty Polymers GPP6100-116C PP Application: Specially engineered, low bloom, low specific gravity, flame retardant polypropylene compound designed with halogen based technology. Exhibits a unique balance of high flexural modulus .. |
|||
Melt Flow | 12 - 20 g/10 min @Load 2.16 kg, Temperature 265 °C |
12 - 20 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Melt Flow | 15 - 20 g/10 min @Load 2.16 kg, Temperature 265 °C |
15 - 20 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D1238 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 11.6 kg, Temperature 250 °C |
14 - 20 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Flow | 10 - 20 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 - 20 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
14 - 20 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Melt Flow | 15 - 20 g/10 min | 15 - 20 g/10 min | ASTM D3275 |
Solvay Specialty Polymers Halar® 558 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Halar 558 fluoropolymer is a resin grade for foam extrusion applications, including primary insulations, coaxial cable cores, cross-webs, fire alarm cable, jackets, and foam tubing. Like other grade.. |
|||
Melt Flow | 15 - 20 g/10 min | 15 - 20 g/10 min | ASTM D1238 |
Kolon KOCETAL® GF702 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties. Information provided by API-Kolon. |
|||
Melt Flow | 10 - 20 g/10 min @Load 2.16 kg, Temperature 150 °C |
10 - 20 g/10 min @Load 4.76 lb, Temperature 302 °F |
|
Taiwan Sheen Soon Sheenthane® AH-783 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for hotmelt adhesiveNon-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized... |
|||
Melt Flow | 12 - 20 g/10 min | 12 - 20 g/10 min | 300/1.2; May be specified; ASTM D1238 |
Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Melt Flow | 15 - 20 g/10 min @Temperature 230 °C |
15 - 20 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Melt Flow | 12 - 20 g/10 min | 12 - 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 10 - 20 g/10 min | 10 - 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Melt Flow | 15 - 20 g/10 min @Temperature 230 °C |
15 - 20 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Melt Flow | 10 - 20 g/10 min | 10 - 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Melt Flow | 15 - 20 g/10 min @Temperature 230 °C |
15 - 20 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Melt Flow | 5.0 - 20 g/10 min @Load 8.70 kg, Temperature 210 °C |
5.0 - 20 g/10 min @Load 19.2 lb, Temperature 410 °F |
|
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in.. |
|||
Melt Flow | 14 - 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
14 - 20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Cresset Powers Cress-Alon™ A2600 2.6 r.v. Compounding Grade Nylon 6, 50% RH Neat resin, for compounding.Information provided by Cresset Powers Ltd. |
|||
Melt Flow | 15 - 20 g/10 min @Load 1.20 kg, Temperature 190 °C |
15 - 20 g/10 min @Load 2.65 lb, Temperature 374 °F |
die 8/1; ISO 1133 |
Addcomp PRIEX® 25097 Maleic Anhydride Grafted PP random copolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, o.. |
|||
Melt Flow | 10 - 20 g/10 min @Load 12.5 kg, Temperature 232 °C |
10 - 20 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Melt Flow | 12 - 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 - 20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® GFPC 5030 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 6.0 - 20 g/10 min | 6.0 - 20 g/10 min | ASTM D1238 |
Buckeye Polymers BP PPC 0510 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Melt Flow | 10 - 20 g/10 min | 10 - 20 g/10 min | ASTM D1238 |
Buckeye Polymers BP PPC 0510-20 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Melt Flow | 12 - 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 - 20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Melt Flow | 10 - 20 g/10 min | 10 - 20 g/10 min | 230/2.16; May be specified; ASTM D1238 |
Plastics Group Polifil® RP-PP Polypropylene, Molding Grade Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de.. |
|||
Melt Flow | 16.1 - 20 g/10 min | 16.1 - 20 g/10 min | A |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |
|||
Melt Flow | 10 - 20 g/10 min @Load 12.5 kg, Temperature 232 °C |
10 - 20 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |