Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 381 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 241RX PC (Europe-Africa-Middle East)
LEXAN 241RX is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.75 mm and allows for the molder to use up to 50 percent regri..
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 244R PC (Europe-Africa-Middle East)
LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also US FDA food contact compliant available in limited colorsThis dat..
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East)
Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen..
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® LS2 PC (Europe-Africa-Middle East)
LEXAN LS2 is a medium viscosity grade especially designed for applications with high optical requirements in terms of clarity and light transmission.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm,
Temperature 23.0 °C
381 kV/in

@Thickness 0.126 in,
Temperature 73.4 °F
Short Time; ASTM D149
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Dielectric Strength 15.0 kV/mm

@Thickness 3.00 mm
381 kV/in

@Thickness 0.118 in
ASTM D149
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz..
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL V03550 PPE+HIPS
Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Dielectric Strength 15.0 kV/mm

@Thickness 3.00 mm
381 kV/in

@Thickness 0.118 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS)
High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2100R PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2110R PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with ..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Dielectric Strength 15.0 kV/mm

@Thickness 3.18 mm
381 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU)
Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins...
Dielectric Strength 15.0 kV/mm

@Thickness 3.18 mm
381 kV/in

@Thickness 0.125 in
ASTM D149
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU)
Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East)
VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East)
VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light..
Dielectric Strength 15.0 kV/mm

@Frequency 60.0 Hz
381 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bakelite North America, Inc.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm,
Temperature 200 °C
381 kV/in

@Thickness 0.126 in,
Temperature 392 °F
Short Time; ASTM D149
DuPont Performance Polymers Rynite® 830ER NC010 PET
Rynite® 830ER is 30% glass reinforced with excellent high temperature dielectric properties. Class H (180C).Information provided by DuPont Performance Polymers
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East)
LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors.
Dielectric Strength 15.0 kV/mm

@Thickness 1.00 mm
381 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East)
Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc..
Dielectric Strength 15.0 kV/mm

@Thickness 3.20 mm
381 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East)
VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes.