Plastcom SLOVAMID 66 OB PA66, optically brightened

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 OB PA66, optically brightened.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 66 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and modulus of elasticity in tension in comparison with the basic type. The microcrystal structure guarantees the isotropy of mechanical properties. Use in the engineering and electrical industry. Delivered in natural mode.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Viscosity Measurement 1.8 - 1.93
1.8 - 1.93
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
Linear Mold Shrinkage, Transverse 0.0193 cm/cm
0.0193 in/in
Melt Flow 4.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
4.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
Elongation at Break 3.5 %
3.5 %
Tensile Modulus 3.50 GPa
508 ksi
Flexural Strength 120 MPa
17400 psi
Flexural Modulus 2.90 GPa
421 ksi
Charpy Impact Unnotched 10.0 J/cm²

@Temperature -20.0 °C
47.6 ft-lb/in²

@Temperature -4.00 °F
11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
Vicat Softening Point 250 °C
482 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 960 °C
1760 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
762 kV/in
Comparative Tracking Index 600 V
600 V
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi