Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 32 B/IM PA6 Basic type PA 6 for injection molding, compounding, for general use. Use: automotive, engineering, electrical and consumer goods industry - electrical tools, fasteners, clamps, hobby tools, toys. De.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 27 B/IM PA66 PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, cla.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT N 27 B/IM PA66 PA66 for injection molding, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, cla.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 FRM1X3 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 T 36 TS PA66, 36% mineral filling FeaturesPA 66 with the content of 36 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 W 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel .. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® B BT BK PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTYR® B BT N PBT Regranulate PBT basic type for injection molding. Melt is characterized by very good fluidity, which enables injection molding of complicated and divided products also on multiple moulds. Anisotropy.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPC TS4030 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T16040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne Bergamid™ B70 GK/Mi30 BK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 92 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packag.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 15 FRA 5 Polyamide 6, 15% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH BK901010 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl PKN4766 PPE+HIPS (Europe-Africa-Middle East) NORYL PKN4766 is a translucent PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulat.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30) 25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRC 2 TS PA6, flame retardant, heat stability FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature -20.0 °C |
0.952 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH TS15030 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.200 J/cm² @Temperature 23.0 °C |
0.952 ft-lb/in² @Temperature 73.4 °F |
|
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion .. |