Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E1501 Polyvinyl Chloride, Rigid (PVC, Rigid) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66 LNP* COLORCOMP* R1000 is an unfilled Nylon 66. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Flexural Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | |
Lehmann & Voss LUVOCOM® 1700-8126 PPO, with glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High dimensionally stable precision parts, even at elevated temperatures and narrow tolerance r.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | Conditioned; ISO 178 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Lucite International Diakon® ST25H8 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Astryn 65F4-4 Polypropylene Homopolymer, 40% Talc Key Features: conventional melt flow, high modulus, mineral-filled polypropylene homopolymer, high stiffness, good dimensional stability, excellent heat resistanceApplications: automotive heater and.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KAL22 is a compound based on Acetal Copolymer resin containing PTFE, Aramid Fiber. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL004AXC Acetal Homopolymer LNP* LUBRICOMP* KL004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP MG004 PP (Europe-Africa-Middle East) LNP* Lubricomp* MG004 is a compound based on Polypropylene resin containing Graphite Powder. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Solvay Technyl® C 217 Unfilled, Heat Stabilized, Impact Modified Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon DS0029 PC (Asia Pacific) LNP STAT-KON* DS0029 is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MK0049A PP (Europe-Africa-Middle East) LNP* STARFLAM* MK0049A is a compound based on Polypropylene resin containing Talc, Flame Retardant. Added features include : Flame Retardant. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Polyram PlusTek PA201 Nylon 66 for Extrusion High viscosity Nylon 66 for extrusion applications.Information provided by Polyram. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178-93 |
Wellman Wellamid® 22LH-NBK4/WE1657 Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | cond; ISO 178 |
DSM Novamid® 1013G15 1 NA PA6-GF15 15% Glass Reinforced, Injection Molding |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions... |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant designed for low wear and fr.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Cossa Polimeri ESTABLEND PA 1424 GF HI ABS / Nylon 6 Blend, 12% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.12% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Flexural Modulus | 2.90 - 15.2 GPa @Temperature -40.0 - 150 °C |
421 - 2200 ksi @Temperature -40.0 - 302 °F |
Average value: 8.35 GPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |