Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Linear Mold Shrinkage 0.0145 cm/cm
0.0145 in/in
Linear Mold Shrinkage, Transverse 0.0155 cm/cm
0.0155 in/in
Melt Flow 2.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
2.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
Elongation at Break 6.0 %
6.0 %
Tensile Modulus 3.80 GPa
551 ksi
Flexural Strength 50.0 MPa
7250 psi
Flexural Modulus 3.90 GPa
566 ksi
Charpy Impact Unnotched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
3.00 J/cm²

@Temperature 23.0 °C
14.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Vicat Softening Point 160 °C
320 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content <= 0.20 %
<= 0.20 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi