Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.90 GPa | 566 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | |
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade Information provided by Polykemi AB |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Shell Carilon® DB6G3A10 Polyketone, 15% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G3A10 is a 15 percent short glass-fiber-reinforced general-purpose injection molding grade with .. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Flexural Modulus | 3.90 GPa @Temperature 23.0 °C |
566 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Flexural Modulus | 3.90 GPa @Temperature 60.0 °C |
566 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | |
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
M. Holland Company SA311 Styrene Acrylonitrile Medium clarityGood processabilityHigh stiffnessApplications: AppliancesCosmeticsHousehold goods |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC LNP THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Polyplastics Duranex® 6300B Polybutylene Terephthalate (PBT), Anisotropy improvement, 30% GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178-93 |
Wellman Wellamid® GFT1699-WBK1 13% Glass Fiber Reinforced, Weatherable Black Nylon 66 Description: Glass Fiber Reinforced, Weatherable Black Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
Clariant ABS4500G10BK ABS, 10% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 621 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 3.90 GPa @Temperature 160 °C |
566 ksi @Temperature 320 °F |
ISO 178 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
Panjin Zhongrun Chemerize 021P Medium Viscosity CoPEEK Information provided by Bieglo Gmbh. |