Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A CV300LK (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -40.0 °C |
14.3 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid FGFHUV-30 Polyamide 6, 30% Glass Fiber Reinforced with glass fiber. Heat and UV stabilized, for long-lasting use at 120-140°C, resistant to artificial light.Information provided by Qualchem Zrt. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® S224-KMV7 Nylon 66-35% Mineral Reinforced (European and Asian Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Inno-Comp INNOPOL® CS 2-4120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-4120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form as well.INNOPOL® CS 2-4120 is developed for p.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls PA6, molding grade, micro glass balls, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® KU 1-7313 000000 PBT + PET, 15% Glass Fiber PBT+PET, 15% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific) Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Akulon® K224-LGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eU |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Arnite® TV4 220 PBT-10% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eU |
Eurotec® Tecodur® PB70 KK45 NL XA 20 PBT 45% glass fiber/mineral reinforced, UL94 V0, low warpage Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultradur® B 4406 G2 10% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 10% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® 9H TES/30 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Aesthetic talc.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |