Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 160 °C | 320 °F | B |
Plastcom SLOVALEN PH 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards oxidants. General application in all industry branches -.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Vicat Softening Point | 160 °C | 320 °F | B; STN EN ISO 306 |
Plastcom SLOVALEN PH 91 T 20 Polypropylene Homopolymer, 20% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound
(Unverified Data**) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 80-7713 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Vicat Softening Point | 160 °C | 320 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Vicat Softening Point | 160 °C | 320 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Vicat Softening Point | 160 °C | 320 °F | ISO 306 |
Suzhou Hipro Polymers Hiprolon® 11 PES Colorized Nylon powder Hiprolon® 11 PES colorized electrostatic polyamide powder is partly comprised of bio-renewable raw materials. It has excellent weather ability, chemical resistance, wear resistance, impact resist.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)
(Unverified Data**) 10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/h 50N; ISO 306 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Vicat Softening Point | 160 °C | 320 °F | B/120; ISO 306 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Arkema Group Rilsan® BESN TL Nylon 11, Rigid Tubing Grade (Conditioned) Designation ISO 1874-PA11,EHL,22-010Rigid grade for tubes extrusion. Available colors: black and natural. Light and heat stabilized.High impact strength. High burst pressure. Good chemical resistanc.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Arkema Group Rilsan® Powder T NAT BHV COS Nylon 11, Cosmetic Grade Powder T NAT BHV COS - RILSAN POLYAMIDE 11 (PA11) POWDERUnpigmented and clear Powder for the cosmetic industry, used as mild abrasive in 'scrubbing' creams.The properties listed in the dat.. |
|||
Vicat Softening Point | 160 °C | 320 °F | 50°C/hr; 50N |
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |
|||
Vicat Softening Point | 160 °C | 320 °F | ISO 306/A50 |
Addiplast Addilene H 511 V30 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Vicat Softening Point | 160 °C | 320 °F | |
BASF Luranyl® KR 2460/3 Polyphenylene Ether + Styrene-Butadiene Blend Flame retardant grade with very high heat resistance; used for precision parts and where the material must withstand high injection temperatures (e.g. heater-fan impellers).Data was collected by ISO.. |